ABSTRACTA magnetic refrigeration test was performed using a test device filled with spherical GdN material synthesized by the hot isostatic pressing (HIP) method. Refrigeration with an active magnetic regenerator cycle was tested in the temperature range between 48 and 66 K, with the field changing from 1.2 to 3.7 T and 2.0 to 4.0 T at upper and lower sides of the regenerator bed filled with the GdN spheres, respectively. Temperature spans about of 2 K were obtained at both sides, and the total temperature span in each cycle attained about 5 K. The specific heat of the material was measured to calculate the magnetic entropy change ΔS and the adiabatic temperature change ΔT induced by the magnetic field change ΔH. It was suggested that for a given ΔH, larger ΔS and ΔT can be exploited when demagnetized to lower H, especially, to zero field.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.