Magnetic properties of the synthesized solid solution x FeTiO 3 ·(1- x ) Fe 2 O 3 of ilmenite (FeTiO 3 ) and hematite (Fe 2 O 3 ) were investigated in detail for the whole range of 0≦ x ≦1. On the experimental side of the study, the most suitable method for preparing the specimen with the largest intensity of magnetization was found. Changes of the Curie point, the estimated intensity of magnetization at 0°K, the Curie constant and the asymptotic paramagnetic Curie point with the composition were presented. It was found that the magnetic properties of the solid solution, x FeTiO 3 ·(1- x )Fe 2 O 3 , could be divided into three parts, (i) x =1, (ii) \(1>x{\gtrsim}0.5\) and (iii) 0.5> x ≧0: Pure ilmenite (FeTiO 3 ) is antiferromagnetic below 55°K and the specimens for \(1>x{\gtrsim}0.5\) are very strongly ferromagnetic and for 0.5> x ≧0 they are again antiferromagnetics on which feeble parasitic ferromagnetism is superimposed. On the theoretical side of the study, these magnetic properties were discussed by...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.