The element-selected magnetic circular dichroism (MCD) between Gd core states is observed in the soft X-ray region (1150-1250 eV). The dichroism intensity for the transition from the 3d to 4f orbital of the Gd atomic state is very strong and reaches up to about 30% at 15 K. The temperature dependence of the MCD intensity shows a ferromagnetic phase around 50-80 K in addition to the room temperature ferromagnetic phase. Its X-ray absorption near edge structure is different from those of other Gd compounds. It seems to be related to the strength of the ferromagnetic behavior.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.