Co 79.6 Fe 4.6 Si 9.2 B 2.7 Mo 3.9 fibers have been produced by the modified process of melt-extraction. Hysteresis loop, magnetostriction constant, λ s and giant magneto-impedance (GMI) ratio (total impedance, real and imaginary contributions) of such fibers have been measured. Studied fibers exhibit excellent magnetic softness (coercivity about 20 A m −1 ), small positive magnetostriction constant ( λ s ≈1.13×10 −6 ) and GMI ratio of the order of 50% in as-cast state. Current annealing has been employed to tailor the magnetic properties and GMI effect of these fibers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.