Magnetic phase transition characteristic in La0.7Sr0.3MnO3/Ta2O5 composites with different grain size was investigated in this work. There were double maxima in |dM/dT|–T curves for the composites with grain size in the range of 100–200nm sintered at relative low temperature for short time, which indicated that two paramagnetic–ferromagnetic (PM–FM) transitions happened. The PM–FM transition temperatures of Tc1 and Tc2 were the contribution of grain boundary and grain, respectively. Tc1 varied with Ta2O5 content and sintering condition, whereas Tc2 remained almost the same value. For the composites with grain size larger than 500nm sintered at high temperature for long time, single magnetic phase transition behavior was observed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.