Abstract

Hiperco® 50 alloy heat treated between 450 and 650 °C exhibits superior mechanical properties. We report the measurements of the ac core loss at various frequencies up to 4500 Hz of the Hiperco® 50 alloy samples annealed at 450 and 650 °C. The 650 °C annealed specimens have lower ac core loss than that of the 450 °C annealed ones. The total core loss, consisting of contributions from hysteresis core loss and eddy-current core loss, depends on frequency f as af+bf2. The eddy-current loss of a single laminate is minor compared to the hysteresis loss.