Strontium ferrite was incorporated into different rubber matrices to prepare rubber magnetic composites. Three types of elastomers, butadiene rubber BR as non‐polar elastomer, acrylonitrile butadiene rubber NBR and blend acrylonitrile butadiene rubber–polyvinyl chloride NBR/PVC as polar elastomers were chosen as rubber matrices. Surface modified strontium ferrite as magnetic filler was applied in concentration scale ranging from 0 to 100 phr. Besides the rubber and the filler, the rubber compounds contained only the ingredients of sulfur curing system. The results revealed that thermo‐physical and magnetic properties of composites increased with doping content of ferrite. Moreover, the improvement of mechanical properties in dependence on strontium ferrite content was also recorded. It can be stated that the improvement of composite properties is in close correlation with the increase of polarity of the rubber matrix. POLYM. COMPOS., 38:2480–2487, 2017. © 2015 Society of Plastics Engineers

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.