This paper reported three acid (including hydrochloric acid HCl, p-toluenesulfonic acid PTS and D-camphor-10-acid CSA) doped SrPr0.2Fe11.8O19/PANI composite film and the HCl–PANI film prepared by a sol–gel method and in-situ oxidative polymerization. The characteristics of the film phase structure, surface morphology, conductivity and magnetic and electromagnetic properties were studied by using XRD, XPS, FESEM, four-probe tester, VSM and Vector Network Analyzer. The resistivity of organic acid doped composite films is higher than that of the HCl doped one. The saturation and remanent magnetization of PTS and HCl doped composite films are greater than the CSA-doped one; however, the coercivity of the three acid doped composite films is basically 5546Oe. The saturation magnetization, remanent magnetization and coercivity of SrPr0.2Fe11.8O19 film are greater than those of the SrPr0.2Fe11.8O19–PANI composite film. In the frequency range of 8–12GHz, the dielectric loss of HCl–PANI film is the maximum, and the dielectric loss of SrPr0.2Fe11.8O19 film is the minimum; the magnetic loss of the four films is in descending order as SrPr0.2Fe11.8O19 film, PrSrM/(HCl–PANI) composite film, PrSrM/(CSA–PANI) and HCl–PANI film.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.