Abstract

The after-effect of permeability μ in amorphous Fe 40 - Ni 40 - P 14 - B 6 and Fe 80 - B 20 was studied during 1.5 h annealings between −70 and 140°C. A μ decay almost linear with the logarithm of time is observed, which must be described by a superposition of processes with a broad activation energy spectrum.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.