Abstract

Mg was reinforced with SiC nanoparticles by powder metallurgical technique. The SiC nanoparticles were generated by laser-induced gas phase reaction in a flow reactor and had a median particle diameter of 30 nm. In order to distribute the nanoparticles in the Mg matrix, Mg micropowder with a median particle diameter of 40 μm was mixed or ball milled with the nanoscaled ceramic powder followed by hot extrusion. The mechanical properties of the new material were investigated by tensile tests and creep measurements and the microstructure of the composites were examined by light and transmission electron microscopy (TEM).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.