The solvent extracts of Upper Freeport and Illinois No.6 coals were mixed with N-methyl-2-pyrolidinon (NMP) and annealed at 353 K to produce the gelatinous materials. Differential scanning calorimetric measurements revealed that the materials can hold significant amounts of nonfreezable NMP (as much as 3 g NMP per 1 g coal extracts) which disperse in the materials on a molecular scale, indicating the materials are not phase separated. The thermal behaviors were measured macroscopically as a function of the extract concentration using a needle penetrometer during heating from 223 to 360 K. The penetration–temperature curves were analyzed to estimate the apparent viscosity ( η a). During the penetrations, η a was decreased very rapidly, approximately four orders of the magnitude by a temperature increase of 20 K, suggesting that the coal extracts-NMP mixtures undergoes a gel to sol transition. The heats of dissociation of crosslinks (Δ H m) were estimated by applying Eldridge–Ferry equation. The Δ H m of coal extracts-NMP mixtures was relatively small, i.e. approximately 10 kJ/mol, whereas the Δ H m of polyvinyl alcohol-NMP gel in which the hydrogen bonds contribute the formation of the physical network structures, was about 65 kJ/mol. Not the specific interaction such as hydrogen bonds, but weak interactions such as van der Waals force were likely to contribute the formation of the coal extracts-NMP gel.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.