Single-crystal superalloys are typical advanced materials used for manufacturing aeroengine turbine blades. Their unique characteristics of high hardness and strength make them exceedingly difficult to machine. However, a key structure of a turbine blade, the film-cooling hole, needs to be machined in a single-crystal superalloy; such machining is challenging, especially considering the increasing levels of machining efficiency and quality demanded by the aeroengine industry. Tube electrode high-speed electrochemical discharge drilling (TSECDD), a hybrid technique of high-speed electrical discharge drilling and electrochemical machining, provides high machining efficiency and accuracy, as well as eliminating the recast layer. In this study, TSECDD is used to machine a film-cooling hole in a nickel-based single-crystal superalloy (DD6). The Taguchi methods of experiment are used to optimise the machining parameters. Experimental results show that TSECDD can effectively drill the film-cooling hole; the optimum parameters that give the best performance are as follows: pulse duration: 12μs, pulse interval: 30μs, peak current: 6A, and salt solution conductivity: 3mS/cm. Finally, a hole is machined by TSECDD, and the results are compared with those obtained by electrical discharge machining. TSECDD is found to be promising for improving the surface quality and eliminating the recast layer.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.