The luminescent characteristics of K3LuSi2O7:Pr3+ (1%), which is a promising optical material for the use as a scintillator, have been studied using a set of techniques. The luminescence spectra of K3LuSi2O7:Pr3+ (1%) contain two bands in the UV-range with peaks at 284 and 330 nm, which correspond intraconfigurational 5d → 4f transitions in the Pr3+ ions. The radiation in the visible and near IR range (480–850 nm) has been represented by the intraconfigurational 4f → 4f transitions. The kinetics of 5d → 4f-luminescence contains a build-up stage (τrise ∼ 7–12 ns), nonexponential decay stage (τ1/2 ∼ 60 ns), and a slow component of the μs-range when excited by high-frequency (∼8 MHz) synchrotron radiation of the X-ray range. The fast component of the decay (τ = 54 ns) dominates in the decay kinetics of luminescence along with the build-up stage while the contribution of the μs decay component is less than 0.5% at the excitation by an pulse electron beam (5Hz). The excitation spectra of d–f- and f–f-photoluminescence in the ultraviolet and vacuum ultraviolet range that are measured using synchrotron radiation reveal features that are caused by both intracenter transitions and processes related to the energy transfer from the intrinsic electronic excitations to the impurity center.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.