AbstractSpinel‐type ZnGa2O4 and ZnAl2O4 powders doped with Eu3+ and Tb3+ ions, including dual doping, have been prepared by solid phase reactions and by deposition from chemical solutions. XRD analysis demonstrates the high quality of spinel grains constituting the powder. The luminescence shows that the rare earth ions are incorporated in the defect regions at the grain boundaries. The emission spectra of the samples with europium are characterized by an intense emission in red region due to the 5D0 → 7F1,2 transitions of Eu3+ ions, whereas in the case of terbium the highest intensity corresponds to the green emission due to the 5D4 → 7F5 transitions of Tb3+ ions. The possibility to change the color of the emission from green to red by the variation of Tb and Eu doping concentration is demonstrated. (© 2009 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.