Mg0.5Ti2(PO4)3:Dy3+/Eu3+ phosphors were prepared via solid-state reaction method under normal ambient air. The phosphors were characterized by X-ray, photoluminescence excitation and emission spectra. The XRD patterns showed that Dy3+ and Eu3+ could be effectively doped into the Mg0.5Ti2(PO4)3 host. The concentration quenching mechanism of Dy3+ in the Mg0.5Ti2(PO4)3 host was proven to be dipole-dipole interaction. The emission intensity and the decay lifetime of Dy3+ decreased with the increase of Eu3+ concentration, which proved the existence of the energy transfer from Dy3+ to Eu3+ in the Mg0.5Ti2(PO4)3 host. It was found that the energy was transferred from 4F9/2 level of Dy3+ to the 5D0 level of Eu3+ by dipole-dipole interaction. Besides, the correlated color temperature is improved with the introduction of Eu3+ ions. The experiment presents that Mg0.5−x−yTi2(PO4)3:xDy3+, yEu3+ phosphors are promising materials for warm white UV LEDs.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.