Zinc oxide ZnO micropatterns were synthesized site-selectively on photocatalytically activated regions of TiO2 in an aqueous solution of zinc nitrate and dimethylamine-borane at 55°C by an electroless deposition process. The as-deposited ZnO micropatterns showed a polycrystalline wurtzite structure with a thickness of approximately 0.1 m. The ZnO micropatterns emitted ultraviolet light at 380 nm due to the recombination of bound excitons and broad visible-light luminescence 500-800 nm . © 2005 The Electrochemical Society. DOI: 10.1149/1.1960042 All rights reserved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.