Abstract
Al2O3 films were deposited by atomic layer deposition (ALD) at temperatures as low as 33 °C in a viscous-flow reactor using alternating exposures of Al(CH3)3 (trimethylaluminum [TMA]) and H2O. Low-temperature Al2O3 ALD films have the potential to coat thermally fragile substrates such as organic, polymeric, or biological materials. The properties of low-temperature Al2O3 ALD films were investigated versus growth temperature by depositing films on Si(100) substrates and quartz crystal microbalance (QCM) sensors. Al2O3 film thicknesses, growth rates, densities, and optical properties were determined using surface profilometry, atomic force microscopy (AFM), QCM, and spectroscopic ellipsometry. Al2O3 film densities were lower at lower deposition temperatures. Al2O3 ALD film densities were 3.0 g/cm3 at 177 °C and 2.5 g/cm3 at 33 °C. AFM images showed that Al2O3 ALD films grown at low temperatures were very smooth with a root-mean-squared (RMS) roughness of only 4 ± 1 A. Current−voltage and capacitance−voltage...
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.