Abstract

Ti 3AlC 2 was rapidly synthesized by pulse discharge sintering Ti/Al/C (molar ratio 3:1.1:1.8) powder mixtures in a temperature range of 1200–1400 °C. The fully dense and single-phase Ti 3AlC 2 was obtained at sintering temperature 1250–1350 °C for 15 min and at 1300 °C for 15–60 min. The typical microstructure of polycrystalline bulk Ti 3AlC 2 consists of plate-like grains, and the grain size can be adjusted by choosing sintering temperature and time. The intermediate phases of AlTi 3, AlTi, Ti 3AlC and Ti 2AlC were found during the reactive sintering process and the mechanisms for the Ti 3AlC 2 phase formation were proposed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.