Using tetraethyl orthosilicate and anhydrous aluminum chloride as precursors, ethyl ether as oxygen donor, LiF as mineralizer, and Na2SO4-NaCl as compound molten salt, mullite whisker was synthesized in the low temperature by nonhydrolytic sol-gel process combined with molten salt method. The phase transformation of mixed powder composed of mullite xerogel and molten salt during the heat treatment and the microstructure of mullite whisker corresponding to different temperature were characterized by means of DTA-TG, XRD SEM and TEM. The results show that mullite crystal phase can be formed via non-hydrolytic sol-gel process combined with the molten salt method at 750°C. The synthetic effect of mullite get better as the temperature increased to 850°C, while NaAlSiO4 crystal phase is also detected. Mullite whisker, with diameters ranging from 300~500 nm and lengths of 3~5μm, is prepared at the temperature of 850°C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.