Abstract

The specific heat and thermoelectric power of the UCu 3M 2Al 7 alloys where M = Cr, Mn and Fe are presented. The specific heat has been measured in the temperature range 2.6–70 K in magnetic field H = 0 and 3 T using a homemade and full automatic calorimeter, whereas the thermoelectric power has been measured from 6 to 300 K employing a differential method with copper as reference material. The temperature dependence of the specific heat exhibits only a minute influence of magnetic field and no anomaly in the investigated temperature region. However, the coefficients of the electronic specific heat of all alloys are very close, being enhanced amount to about 200 mJ mol −1 K −2 at high temperature and to about 400 mJ mol −1 K −2 at low temperature. Strongly correlated electrons or crystallographic disorder are considered as a reason for these values. The thermoelectric power demonstrates moderate values within whole investigated temperature range.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.