Abstract
45S5 Bioglass® powder has been densified at low temperatures using Spark Plasma Sintering (SPS). By employing SPS with pressures ranging from 70 to 300MPa, it was possible to achieve fully dense and completely amorphous 45S5 Bioglass® samples at temperatures as low as 500–550°C. By increasing the sintering temperature up to 600°C the dense samples crystallized to Na2CaSi2O6 phase rather than Na2Ca2Si3O9 which is usually achieved at higher temperature. Acellular in vitro test results in Simulated Body Fluid (SBF) revealed that SPSed samples sintered at 600°C resulted in faster formation of hydroxyapatite compared to pressureless sintered ones (1050°C), which were highly crystallized. Amorphous Bioglass® and/or Na2CaSi2O6 phase prepared by SPS could potentially produce Bioglass® composites with increased bioactivity.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.