AbstractSolution‐based nickel induced crystallization of amorphous silicon (a‐Si) films was performed. The nickel solution was prepared by dissolving (CH3CO2)2Ni in deionized water and applied uniformly on a‐Si films by low‐cost ultrasonic spray pyrolysis method. Crystallization could be realized for a‐Si films coated with a 0.2 M nickel solution and annealed at 500 °C. The effect of substrate temperature during nickel solution deposition was analyzed. Micro‐Raman and x‐ray diffraction measurement show that a‐Si is fully crystallized at 550 °C for 7 h with a nickel concentration of 0.8 M. (© 2011 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.