Abstract
Beryllium oxide (BeO) is a unique metal oxide that exhibits high thermal conductivity and a high dielectric constant, even though it has a large bandgap energy. These characteristics can potentially address the electromagnetic issues associated with contemporary nanoscale electronic devices. However, BeO is mainly used as a heat-dissipating and refractory layer in sintering powders. To extend the use of BeO in semiconductor front-end-of-line processes, we developed nanoscale BeO thin films by using state-of-the-art atomic layer deposition (ALD). The physical and electrical properties of the BeO thin films were evaluated by introducing O2 plasma and H2O vapor as oxidation sources for the ALD process. A controlled plasma-enhanced ALD (PEALD) process led to the production of c-axis grown crystalline wurtzite BeO (002) films with a high growth rate per cycle at low substrate temperatures. The plasma energy was found to be adequately compensate for the high substrate temperature required for thermal ALD (ThALD). The bandgap energy (7.9 eV), calculated via inelastic energy loss analysis, and the dielectric constant (8.75) and breakdown voltage (10.3 MV/cm), obtained from MOS capacitors, are optimal for nanoscale electronic device applications.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.