Silicon oxide films have been formed at temperatures as low as 25°C, using a reaction of Si with a vapor mixture containing either NO, HF and H 2O or NO, HF, H 2O and O 2. Experimental data relating silicon oxide film growth with processing parameters such as vapor composition, temperature and time are presented. Conditions for the growth of silicon oxide films of specific thicknesses are outlined.