Abstract
Ultrafine aluminide coatings were successfully produced on Ni–18Fe–17Cr superalloy at 540–600 °C in a modified pack-aluminizing process. Repeated ball-impacts accelerated the formation of the aluminide coatings by a surface refining process, resulting in atomic diffusion occurring at a relatively low temperature. The effects of the operation temperature and the treatment duration on the formation of the coatings have been investigated. The coatings possessed a two-layer structure. The top layer, approximately 5 µm in thickness, exhibited equiaxial coarse grains and was dominated by NiAl 3, with small amounts of Fe 2Al 5 and CrAl 5. The bottom layer showed high density, homogeneous, ultrafine grains with diameters approximately 30–50 nm. High-temperature oxidation tests were carried out at 1000 °C. The oxidation kinetics and microstructure of the oxide scale were studied. The experimental results indicated that the coatings greatly enhanced the high-temperature oxidation resistance of Ni–18Fe–17Cr superalloy.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.