Herein, a reliable diffusion bonding of Ti3Si(Al)C2 ceramic is achieved by applying Au foil as an interlayer at 650 °C for 30 min with an axial pressure of 20 MPa. This novel method significantly decreases the bonding temperature, which is about 150 °C lower than the lowest bonding temperature from current research to the best of our knowledge. Maximum shear strength of 58 MPa is achieved at 650 °C among the bonding temperature range of 600 °C~800 °C. The microstructure evolution mechanism and the relationship between microstructure and mechanical property are discussed. The facile mutual diffusion of Au with de-intercalated Al and Si from Ti3Si(Al)C2 is considered critical in achieving sound interfacial bonding.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.