Abstract

Unexpectedly large amounts of CO adsorption have resulted from a pulse adsorption experiment at 323 K, giving about 300% Pt dispersion in a Pt/cerium-based oxide catalyst. An in situ diffuse reflectance infrared Fourier transform spectroscopic investigation on a Pt/cerium-based oxide during CO adsorption has revealed that carbonate species on the cerium oxide surface are responsible for the unrealistically large CO adsorption at 323 K, as a result of CO spillover. Lowering the temperature to 195 K considerably diminished the amount of CO adsorption. The size of the Pt particles in the Pt/cerium-based oxide catalyst was determined by CO pulse adsorption at 195 K and showed good agreement with the particle size determined by X-ray diffraction and low energy ion scattering. This indicates that CO pulse adsorption at 195 K is a useful technique to reliably estimate the Pt particle size in a Pt/cerium-based oxide catalyst.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call