Abstract

Aluminum-aluminum thermo-compression wafer bonding is becoming increasingly important in the production of microelectromechanical systems (MEMS) devices. As the chemically highly stable aluminum oxide layer acts as a diffusion barrier between the two aluminum metallization layers, up to now the process has required bonding temperatures of 300°C or more. By using the EVG®580 ComBond® system, in which a surface treatment and subsequent wafer bonding are both performed in a high vacuum cluster, for the first time successful Al-Al wafer bonding was possible at a temperature of 100°C. The bonded interfaces of blank Al wafers and Al wafers with patterned frames were characterized using C-mode scanning acoustic microscopy (C-SAM) and transmission electron microscopy (TEM) as well as dicing yield and pull tests representative for the bonding strength. The investigations revealed areas of oxide-free, atomic contact at the Al-Al bonded interface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.