Abstract

Fast and thick 4H-SiC epitaxial growth is demonstrated in a vertical-type reactor under a low system pressure within the range 13-40 mbar. A very fast growth rate of up to 250 m/h is obtained. The material quality of the epilayers grown in the reactor is evaluated by low-temperature photoluminescence, deep level transient spectroscopy, microwave photoconductive decay, synchrotron topography and room temperature PL imaging. The carrier lifetime of thick epilayers with or without the application of the C+-implantation/annealing method and extended defects in the epilayers grown on 8º and 4º off substrates are discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.