Abstract
As high-grade refractories raw material,kyanite is widely used and the market demand is increasingly greater. To identify the process mineralogical properties of kyanite from Heibei so as to provide a mineralogical basis for its chemical composition, mineral constituent,ores texture and structure and so on. The results show that: the kyanite Al2O3 21.50%, SiO2 52.87%, using high intensity magnetic separation-gravity separation-flotation folwsheet. Experiments show that, the grinding fineness of -200 mush 65%, with strong intensity magnetic separation, magnetic concentrate by shaking the low intensity magnetic separation,we can get magnetite, garnet, biotite and phlogopite four concentrates, strong magnetic ore tailings consolidated by a rocking bed mud thrown first, refined through flotation, won Kyanite concentrate grading about 56.11% at a recovery of 49.90%.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.