Fatigue crack path behavior of a series of Ti-Mn alloys heat treated to produce volume fractions of the alpha phase ranging from 0 to 97.5 pct was investigated. Both Widmanstatten and equiaxed morphologies of the α phase were used in this study. Interior and surface crack paths are discussed in terms of slip behavior and microstructural details.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.