Abstract

The feasibility of long-term operation of SOFC is demonstrated with a short-stack with 2 anode supported cells at 700 °C at constant current density of 0.5 A/cm² over 30,000 hours resulting in a degradation rate in the order of 8 mV/kh on average. Reduction of the degradation rate to about 4 mV/kh is shown to be possible by selecting alternative manufacturing methods as for instance atmospheric plasma spraying for the protective coating on interconnect steel.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.