In order to verify the result of theoretical analysis about long-pulse flat-topped multi-Gaussian laser-induced damage in an optical anti-reflection film with HfO2/SiO2 composite film coating on a BK7 substrate (BK7:HfO2/SiO2), an experimental system was built, which carried out the experiment and analysis, focusing on the pulse-length 1.0 ms, flat-topped laser-induced damage. The result shows that the thermal effect is the main reason for damage under the long-pulse flat-topped laser. Moreover, the stripping and shedding occur because of the heating stress of the film happening at an early stage of the laser irradiation. However, the crack happens at laser irradiation termination. The correctness of the theoretical analysis results is verified.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.