Abstract

The longitudinal–transverse extrusion of hollow components from bar is studied. Strength assessment of the blank is discussed. In view of the stress–strain state of the blanks, limits must be imposed on the process in order to maintain the strength of the lateral surface and prevent critical loads on the tool.