Abstract
ABSTRACTThree iron-based to nickel-based austenitic alloys and three copper-based alloys are being considered in the United States of America as candidate materials for the fabrication of high-level radioactive waste containers. The austenitic alloys are Types 304L and 316L stainless steels as well as the high-nickel material Alloy 825. The copper-based alloys are CDA 102 (oxygen-free copper), CDA 613 (Cu-7A1), and CDA 715 (Cu-3ONi). Waste in the forms of spent fuel assemblies from reactors and borosilicate glass will be sent to a proposed repository at Yucca Mountain, Nevada. The decay of radionuclides will result in the generation of substantial heat and in gamma radiation.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.