Abstract
The effect of thermal ageing at 150 ºC on the corrosion behaviour of Scalmalloy® (Al-Mg-Sc-Zr) alloy additively manufactured by laser powder bed fusion (LPBF) is reported for the first time. Samples before and after the thermal treatment exhibit similar results on cyclic polarisation curves, electrochemical impedance measurements in 3.5 wt% NaCl, and tensile and hardness tests. However, electron microscopy characterisation reveals that the application of this temperature for sufficient time causes most of the grain limits to be decorated by Al3Mg2 particles which in turn provokes the sensitization of the alloy to intergranular corrosion processes due to microgalvanic coupling.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.