Abstract
Three types of CeO2-ZrO2 with the same composition (Ce/Zr = 1) were prepared by different methods, exhibited the different oxygen storage/release capacity (OSC). To investigate the relationship between the OSC and the local structure, the Ce and Zr K-edges XAFS spectra for these samples were measured. The features of Fourier transforms of these samples were different from each other. This suggested that the OSC was remarkably exerted by the local structure around Ce and Zr. The quantitative curve-fitting analysis of EXAFS was applied, and it was concluded that homogeneous Ce(0.5)Zr(0.5)O2 solid solution at atomic level exhibited the highest OSC among these CeO2-ZrO2 with the same composition (Ce/Zr = 1).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.