Quantitative characterization of local strain in silicon wafers is critical in view of issues such as wafer handling during manufacturing and strain engineering. In this work, full-field X-ray microdiffraction imaging using synchrotron radiation is employed to investigate the long-range distribution of strain fields in silicon wafers induced by indents under different conditions in order to simulate wafer fabrication damage. The technique provides a detailed quantitative mapping of strain and defect characterization at the micrometer spatial resolution and holds some advantages over conventional methods.