Abstract
ABSTRACTIn this study, we suggest a simple scheme to derive interfacial behavior using combination of nanoindentation and finite element computation. The starting point is the experimental generation of a rectangular grid composed of 32 indentations to measure the exact variation of stiffness across the interface of a bio‐based composite. A finite element simulation of nanoindentation is implemented based on elasto‐plastic material model. An optimization strategy is used to identify the behavior of all phases by matching predicted results to observed mechanical response. Results show that extent of interphase layer has a typical dimension of 8.0 ± 4.9 µm. The optimization strategy based on simplex proves to be efficient to derive the elasto‐plastic behavior of the blend across the interface with a residual value of less than 30 µN. The identification procedure demonstrates that the extent of the interfacial region depends on the measured physical quantity. The contrast across the interface for both Young's and the tangent moduli appear to be more effective than the contrast given by the yield stress. Identified Young's moduli for zein, starch, and interfacial zone are 4.78 ± 0.27, 4.13 ± 0.19, and 3.91 ± 0.17 GPa. Plasticity parameter represented by tangent modulus varies in the same order as 1238 ± 120, 847 ± 108, and 976 ± 94 MPa, respectively. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2017, 134, 44891.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.