Abstract
High-resolution near-edge x-ray absorption fine structure (NEXAFS) at MnK edge is employed to probe the local environment of Mn dopant in ZnO. First-principles supercell calculations are systematically made to obtain theoretical NEXAFS. Mn is found to substitute for Zn up to 5at.%Mn in polycrystalline samples sintered at 1623K in air. Presence of Mn3O4 is apparent for samples with higher Mn content. The NEXAFS does not change in the range of Mn concentration from 0.01 to 5at.%, indicating the absence of Mn precipitates. The results are confirmed by examining the polarization dependence of the NEXAFS for a 5at.%-doped ZnO thin film.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.