Abstract

The purpose of this in vitro study was to compare the load-bearing capacity of posterior three-unit fixed dental prostheses (FDP) produced with three different all-ceramic framework materials: glass-infiltrated alumina (ICA), glass-infiltrated alumina strengthened with zirconia (ICZ), and yttria-stabilized polycrystalline zirconia (YZ). Additionally, the influence on aging of mechanical cyclic fatigue loading and thermal cycling in water were evaluated. A total of 20 frameworks each were fabricated from ICA, ICZ, and YZ by a computer-aided design (CAD)/computer-aided manufacturing (CAM) system. The framework designs were identical for all specimens. All frameworks were veneered with porcelain and cemented with glass-ionomer. Prior to fracture testing, 10 FDP of each experimental group were subjected to thermal and mechanical cycling. Additionally, fractographic analysis was performed. Statistical analysis showed that FDP made from YZ had significantly higher load to failure, whereas no difference was found between the other two materials. Aging did not have a significant effect on the fracture load.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.