Lithium silicide (LixSi) is the lithiated form of silicon, one of the most promising anode materials for the next generation of lithium-ion batteries (LIBs). In contrast to silicon, LixSi has not been well studied. Herein we report a facile high-energy ball-milling-based synthesis of four phase-pure LixSi (x = 4.4, 3.75, 3.25, and 2.33), using hexane as the lubricant. Surprisingly, the obtained Li3.75Si phase shows significant downward shifts in all X-ray diffraction peak positions, compared with the standard. Our interpretation is that the high-energy ball-mill-synthesized Li3.75Si presents smaller internal pressures and larger lattice constants. The chemical-stability study reveals that only surface reactions occur after Li4.4Si and Li3.75Si are immersed in several battery-assembly-related chemicals. The thermal-stability study shows that Li4.4Si is stable up to 350 °C and Li3.75Si is stable up to 200 °C. This remarkable thermal stability of Li3.75Si is in stark contrast to the long-observed metastability for electrochemically synthesized Li3.75Si. The carbon encapsulation of Li4.4Si has also been studied for its potential applications in LIBs.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call