Abstract

We report on solid state 7Li NMR measurements of electrochemically lithiated SnO. At low Li contents (Li/SnO≤2), the results are consistent with the formation of amorphous Li 2O. For Li/SnO ratio of 4.3, in addition to the amorphous Li 2O phase, there are at least two distinct Sn/Li alloy environments which are similar to those observed in a reference Li 2.3Sn alloy. However the Li + environments in a sample with Li/SnO ratio equal to 6.4 and an Li 4.4Sn reference alloy differ markedly. The NMR data are thus consistent with the simple model of Li insertion proposed by other groups, involving the formation of Li 2O and Li x Sn alloys (SnO+ xLi→Li 2O+Li x−2 Sn), at low and intermediate Li contents. At high Li content, however, the Li x−2 Sn alloy structure is significantly different in the electrochemically lithiated SnO material, compared to that in the reference alloy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.