TlBa 2Ca 2Cu 3O x (Tl-1223) powder was synthesized in O 2 from a mixture of Tl 2O 3 and Ba 2Ca 2Cu 3O x. The peritectic melting point of Tl-1223 in O 2 is 905°C. It was found that the maximum phase conversion to the Tl-1223 phase occurred at 895–900°C. A small concentration of liquid was present at that temperature. Because of the rapid kinetics of Tl-1223 formation, CaO and BaCuO 2 phases became isolated from the Tl 2O 3 and thus remained in the final microstructure. In samples heated at 895°C, the CaO and BaCuO 2 proved to be sufficiently small to act as flux-pinning sites.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.