Despite the ultrahigh intrinsic strength of multiwalled carbon nanotube (MWCNT), the strengthening effect on ceramic matrix composite remains far from expectation mainly due to the weak load transfer between the reinforcement and ceramic matrix. With the assistance of the in situ pullout test, it is revealed that the liquid‐phase sintering (LPS) can serve as a novel strategy to achieve effective load transfer in MWCNT reinforced ceramic matrix composites. The YAlO3 formed liquid phase during spark plasma sintering of SiC composite greatly facilitates radical elastic deformation of MWCNT, leading to highly increased interfacial shear strength (IFSS) as well as interlayer shear resistance (ISR) of nested walls. The liquid phase with superior wettability can even penetrate into the defects of MWCNT, which further increases the ISR of MWCNT. Moreover, the first‐principles calculation indicates that the oxygen terminated YAlO3 phase displays much stronger bonding compared with SiC matrix, which is also responsible for the large IFSS in the composite. As a result, as high as 30% improvement of bending strength is achieved in the composite with only 3 wt% MWCNT in comparison to the monolithic ceramic, manifesting the unprecedented strengthening effect of MWCNT assisted by LPS.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.