Abstract

This study investigated the feasibility of using waste liquid crystal display (LCD) glass powder as a partial replacement for the silica flour that is typically used as a filler in ultra-high-performance concrete (UHPC). In this study, 50% of the silica flour was replaced with LCD glass powder, and its effects on the interfacial bond properties of two steel fiber shapes—circular and triangular—were evaluated. The test results indicated that the LCD glass powder effectively enhanced the bond between the steel fibers and the UHPC, which created a denser interfacial zone; this could be attributed to the filling effects of the LCD glass powder and secondary hydrates. The use of the LCD glass powder increased the pullout energy by 15–40% and the average bond strength by 16%, along with formation of additional scratches on the fiber surfaces. For the same matrix, as compared to the circular steel fibers, the triangular steel fibers yielded superior pullout resistance owing to their higher intrinsic fiber efficiency ratio. Thus, the highest average bond strength and pullout energy of 11.2 MPa and 744 mJ could be obtained from the UHPC mixture containing the LCD glass powder and triangular steel fibers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.