We report on the use of the atomic layer deposition (ALD) process for fabricating liquid core antiresonant reflecting optical waveguides (ARROWs). The ALD permits the deposition of a very conformal sub-100-nm titanium dioxide antiresonant layer. This results in a low loss liquid core ARROW waveguide with a broadband output transmission spectrum. Optical transmitted spectrum from the fabricated structure has been reported, and the measured attenuation losses agree with the theoretical predictions.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.