Abstract
Rene 80 samples were creep–rupture tested in air between 1144 and 1255 K at various stress levels. The mean stress exponent, n, and the mean activation energy for creep were calculated from the experimental results. The accelerated creep life of the alloy was evaluated by using iso-stress parametric equations and Monkman–Grant method.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.