Abstract

Floating-zone growth of untwinned single crystal of ${\text{Li}}_{x}{\text{Cu}}_{2}{\text{O}}_{2}$ with high Li content of $x\ensuremath{\sim}0.99\ifmmode\pm\else\textpm\fi{}0.03$ is reported. Li content of ${\text{Li}}_{x}{\text{Cu}}_{2}{\text{O}}_{2}$ has been determined accurately through combined iodometric titration and thermogravimetric (TGA) methods, which also ruled out the speculation of chemical disorder between Li and Cu ions. The morphology and physical properties of single crystals obtained from slowing-cooling and floating-zone methods are compared. The floating-zone growth under $\text{Ar}/{\text{O}}_{2}=7:1$ gas mixture at 0.64 MPa produces large area of untwinned crystal with highest Li content, which has the lowest helimagnetic ordering temperature $\ensuremath{\sim}19\text{ }\text{K}$ in the ${\text{Li}}_{x}{\text{Cu}}_{2}{\text{O}}_{2}$ system.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.