Abstract

Solvent debinding is one of the processes widely adopted by the powder injection molding industry. Despite the inherent advantages of short debinding cycles, the low temperature employed, and the low investment in processing equipment, dimensional control is still a challenge to the further promotion of this technology. The objective of this study was to investigate the causes of the tolerance-control problems by measuring the in-situ dimensional change and deformation behavior of powder injection-molded (PIM) specimens during debinding, using a self-designed laser dilatometer. Swelling and sagging were found when compacts were immersed in the solvent. Three major factors were found to be responsible for the expansion of the specimens: dissolution of soluble binder into the solvent, reaction between the insoluble binder and solvent, and thermal expansion due to the temperature rise from the solvent bath. The amounts of expansion and sagging were related to the thickness of the sample, the amount of the binder, and the temperature employed. These in-situ measurements on the dimensional change help explain how defects such as slumping, cracking, and distortion come about during debinding and provide some guidelines in selecting processing parameters and in designing binder compositions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.